Glacier Texture Art Glass

Reference Price:USD/㎡
Brand:WEISHENG GLASS
Material No.:EKH65P0A
Supplier: CONTACT USCONTACT US
Material ID:
Add to Project
Material Consultation
Overview
Product Reports
Documents
Specifications
Product Model:ws606223
Country of Origin:Guangdong Province, China
Overall Thickness:16
Flammability:A1
Surface Sheen:Ripple
Color:
Gray Series
Brand Name:WEISHENG GLASS
Series Name:Fused
Category:Glass/Laminated Glass/Woven Laminated Glass
Customizable:Yes
Overview
Structural Diagram
Structural Diagram
Case Diagram
Case Diagram

Details

· Category: Woven wire laminated heat-fused glass (also known as fused wire glass).

· Technique: Under high-temperature heat-fusing conditions, metal mesh or special fiber textures are embedded between multiple glass layers, then shaped by molds to create a three-dimensional texture resembling water ripples or ice cracks.

· Visual characteristics: Up close, it reveals natural crack patterns similar to stone or mica; from a distance, it presents a chaotic ink-wash effect blending grey-green, ink-black, and grey-white. When light passes through, the internal wire refracts tiny sparkling points, delivering a strong sense of depth, layering, and breathability.

· Suitable styles: Perfect for Wabi-sabi, New Chinese, modern minimalist, and industrial interiors. The top choice for screens and room dividers.

Attention

Although this glass has artistic value, its special craftsmanship requires the following daily care:

· Cleaning tools: Never use steel wool, stiff brushes, or coarse cloths. The textured surface easily traps dust; we recommend using a microfiber soft cloth or a soft sponge.

· Cleaners: Avoid strong acidic or alkaline cleaners (e.g., toilet bowl cleaners). Use a neutral glass cleaner. Spray it on and let it sit for a few seconds, then gently wipe with a damp soft cloth, and finally remove water marks with a dry cloth.

· Scratch prevention: Fused wire glass has overlapping melt ripples. While sturdy, its edges and raised areas are very fragile. Be careful when placing or picking up items to avoid chipping caused by hard objects.

· Temperature control: Heat-fused glass often varies in thickness, so it experiences higher thermal expansion stress than ordinary glass during extreme temperature changes (e.g., direct heating vents in winter or air-conditioning drafts in summer). During installation, leave a 2–3 mm expansion gap on all sides and seal the edges with sealant. Never install it tightly without clearance.

· Installation reminder: For large partitions, the glass must be tempered or laminated and installed by professional technicians using frames. Do not rely on adhesive alone to fix it directly onto a wall without support, as uneven pressure may cause breakage.